Used the mold copper tube and coating of different casting machines

How to use the mold copper plate, mold copper tube and coating of different casting machines?For billet continuous casting, there are many copper mould tubes with TP2. The billet is generally gradually made of chromium zirconium copper copper mould tube, especially the copper mould tube with unequal square billet crystal mold is preferably chrome zirconium…

What are the advantages of the concave-convex crystallizer copper tube and the diamond-type crystallizer copper tube?

What are the advantages of the concave-convex crystallizer copper tube and the diamond-type crystallizer copper tube?At present, continuous casting is developing towards high speed, high operating rate and high quality. The main way to increase the pulling speed is to improve the shape of the inner cavity of the copper tube of the mold, and…

Copper mould tube Coating process and inspection

Copper mould tube Coating process and inspection: Process: The process adopts fluid plating,which is a forced circulation of the plating solution in the copper mould tube.the copper mould tube doesnt directly enter the plating tank during electroplating,and the plating solutioin is depleted during the electroplating process because the heavy metal pollution is reduced. Adopt adding…

Rolling technology for hot-rolled bar and deformed steel bar

Rolling technology for hot-rolled bar and deformed steel bar: In accordance with the production line and rolling technology of customers,our products are designed to match one-strand rolling,two-slitting rolling and three-slitting rolling,three-slitting roling,and four slitting rolling,the cemented carbide composite roll includes K1 finished roller,K2 leder roller,K4 pre-slitting roller,K3 slitting roller with high-speed steel as material,the rolling…

The cemented carbide composite roll water quality requirment

The cemented carbide composite roll water quality requirment:Because of the negative effect of heat corrosion,thermal fatigue and thermal stress,the net-shaped thermal fatigue crack usually appears while the collar working,with the increase of cracks,small parts may come off and even the roll rings is broken.we adopt the cooling method to reduce the bad effect,pervent the cracks…